Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 97000 cP | 97000 cP | Accelerator, RVF #7 sp @ 20 rpm |
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of.. |