Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 92000 cP | 92000 cP | 20 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® KVF PVC PVC Homopolymer Dispersion Resin F-KVF is a medium molecular weight, fine particle PVC homopolymer dispersion which imparts pesudoplastic flow to plastisol in which it is used. Plastisol prepared ut.. |