Polymer Property : Brookfield Viscosity = 8500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity <= 8500 cP
<= 8500 cP
Spindle # 4, rpm 60
Michelman® Michem® Guard 25 Nonionic, polyethylene dispersion
Description: Nonionic, polyethylene dispersionUsage: Michem® Guard 25 is a water based polyethylene dispersion which promotes mar resistance and flatting properties in paint and coating formulati..
Brookfield Viscosity 8500 cP
8500 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Formosa Plastics Formolon® 40 PVC
PVC Copolymer Dispersion Resin F-40 is a vinyl chloride vinyl acetate copolymer dispersion resin with low paste viscosities, excellent heat stability, and rapid fusion characteristics. F-40 has been..