Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 850 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
25% Toluene solution; BAM 922
Kraton® D4150 K (SBS) Linear Block Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..
Brookfield Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
BCC Products DP-11-83 Urethane Adhesive-Slo
DP-11-83 is a low viscosity, quick setting, easy to use adhesive and/or casting material. This product was designed to bond together the MB1200 foam board to create desired dimensions in length, wid..