Physical Properties Metric English Comments
Brookfield Viscosity 8400 cP
8400 cP
RVT Spindle 3 @ 20 rpm
Palm Labs Adhesives TURBO-LOCK SERIES 17-HT Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-HT is a fast curing, GREEN, high temperature, high strength, high viscosity, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical p..
Brookfield Viscosity 8400 cP

@Temperature -40.0 °C
8400 cP

@Temperature -40.0 °F
ASTM D5293
ExxonMobil Mobil Delvac Synthetic ATF
Mobil Delvac Synthetic ATF is a synthetic fluid designed that meets the demanding requirements of modern heavy duty automatic transmissions. The synthetic baseoil composition enables excellent perf..
Brookfield Viscosity 8400 cP

@Temperature -40.0 °C
8400 cP

@Temperature -40.0 °F
ASTM D5293
ExxonMobil Mobil Delvac Synthetic ATF
Mobil Delvac Synthetic ATF is a synthetic fluid designed that meets the demanding requirements of modern heavy duty automatic transmissions. The synthetic baseoil composition enables excellent perf..