Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 8200 cP @Temperature 177 °C |
8200 cP @Temperature 350 °F |
ASTM D1084 |
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP) AFFINITY™ GA 1900 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |