Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | <= 8000 cP | <= 8000 cP | Spindle # 3, rpm 60 |
Michelman® Hydrosize® HP-1632 Polyimide solution Polyimide solutionHydrosize® HP-1632 is a specialty coating and high temperature fiber sizing with excellent adhesion properties and abrasion resistance.Information provided by Michelman® |
|||
Brookfield Viscosity | 8000 - 15000 cP | 8000 - 15000 cP | Base, RVF #6 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP-100 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M |
|||
Brookfield Viscosity | 8000 - 16000 cP | 8000 - 16000 cP | Accelerator, RVF #7 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |