Polymer Property : Brookfield Viscosity = 745000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 745000 cP

@Temperature -26.0 °C
745000 cP

@Temperature -14.8 °F
ASTM D2983
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect..