Polymer Property : Brookfield Viscosity = 72 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 72 - 82 cP

@Temperature 20.0 °C
72 - 82 cP

@Temperature 68.0 °F
DIN S3015/ASTM D445
The Chemical Company VESTINOL® 9 Diisononyl Phthalate, C6H4(COOC9H19)2
Diisononyl Phthalate (DINP) C6H4(COOC9H19)2, is a clear, colorless, and almost odorless liquid chemical. It is soluble in most organic solvents. DINP is primarily used as a PVC plasticizer. As compa..