Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 700000 - 900000 cP | 700000 - 900000 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-215 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |
|||
Brookfield Viscosity | 700000 - 900000 cP | 700000 - 900000 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-215 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |