Polymer Property : Brookfield Viscosity = 68200 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 68200 cP
68200 cP
Accelerator, RVF #7 sp @ 20 rpm
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..