Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 35 - 65 cP | 35 - 65 cP | RVF #1 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |