Polymer Property : Brookfield Viscosity = 60000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 10000 - 60000 cP
10000 - 60000 cP
DOP 60phr, 6RPM; ASTM D1824
LG Chemical PE1311 PVC
General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin..
Brookfield Viscosity 20000 - 60000 cP
20000 - 60000 cP
RTV No. 7, 10 rpm
Dow BETAMATE™ 7000 fast curing polyurethane adhesive component
One component of a room temperature fast curing polyurethane structural adhesive.Information provided by Dow
Brookfield Viscosity 20000 - 60000 cP
20000 - 60000 cP
RTV No. 7, 10 rpm
Dow BETAMATE™ 7050 L Epoxy
One component of a room temperature fast curing polyurethane structural adhesive.Information provided by Dow