Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 6.95 cP | 6.95 cP | Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 180 Series 186A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 186A is low molecular weight homopolymer resin, providing a good balance of fused film physical properties and fusion characteristics. It provides excellent chemical foam characteristics with.. |