Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 6.93 cP | 6.93 cP | One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 120 Series 124A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 124A is low molecular weight resin providing lower gelation and faster fusion characteristics. It provideds good chemical foamability for producing medium to high density foams. It gives good.. |