Physical Properties Metric English Comments
Brookfield Viscosity 580 cP
580 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4019 SBR Latex
ROVENE® 4019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external c..