Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 150000 - 550000 cP | 150000 - 550000 cP | T-bar E @ 5 rpm, Uncured |
3M Scotch-Weld™ GM15 Gasket Maker Anaerobic Adhesive 3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal.. |