Physical Properties Metric English Comments
Brookfield Viscosity 5190 cP

@Temperature -40.0 °C
5190 cP

@Temperature -40.0 °F
ASTM D5293
ExxonMobil Mobil 1 Synthetic ATF
Mobil 1 Synthetic ATF is a multi-vehicle, fully synthetic fluid designed to meet the demanding requirements of modern passenger vehicles.Mobil 1 Synthetic ATF is a multi-vehicle formula recommended ..
Brookfield Viscosity 5190 cP

@Temperature -40.0 °C
5190 cP

@Temperature -40.0 °F
ASTM D5293
ExxonMobil Mobil 1 Synthetic ATF
Mobil 1 Synthetic ATF is a multi-vehicle, fully synthetic fluid designed to meet the demanding requirements of modern passenger vehicles.Mobil 1 Synthetic ATF is a multi-vehicle formula recommended ..