Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 5100 cP @Temperature 25.0 °C |
5100 cP @Temperature 77.0 °F |
|
Loctite® 3108 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |