Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3500 - 4900 cP @Temperature 25.0 °C |
3500 - 4900 cP @Temperature 77.0 °F |
25% Toluene solution; BAM 922 |
Kraton® D1133 K (SBS) Linear Block Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |