Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 4.88 cP | 4.88 cP | Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 120X400 is medium molecular weight resin providing a good balance of fusion temperatures and film physical properties. It gives good chemical foamability for producing medium to high density .. |