Physical Properties Metric English Comments
Brookfield Viscosity 380 cP

@Temperature 25.0 °C
380 cP

@Temperature 77.0 °F
25% Toluene solution; BAM 922
Kraton® D4433 P (SIS) Linear Block Copolymer
Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:..
Brookfield Viscosity 380 cP

@Temperature 200 °C
380 cP

@Temperature 392 °F
Melt
Zeon Chemicals Quintone® G115 Aliphatic Hydrocarbon Resin
C5/C9 type (piperylene and dicyclopentadiene precursor).Information provided by Zeon Chemicals L.P.