Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3750 cP | 3750 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 13-OR Anaerobic Thread Locking Compound TURBO-LOCK 13-OR SERIES is a RED, high temperature, high strength, permanent, oil resistant, anaerobic thread-locking compound. It is highly resistance to heat, vibrations, water, gases, oils, hydro.. |
|||
Brookfield Viscosity | 3750 cP | 3750 cP | Mixed, 1 minute; ASTM D2393 |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |