Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3600 cP @Temperature 23.9 °C |
3600 cP @Temperature 75.0 °F |
|
BCC Products BC 5114 Epoxy Laminating System BC 5114 is a gray low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use abov.. |