Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 200 - 325 cP | 200 - 325 cP | RVF #2 sp @ 20 rpm |
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma.. |
|||
Brookfield Viscosity | 200 - 325 cP | 200 - 325 cP | RVF #2 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh.. |