Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2950 cP @Temperature 23.9 °C |
2950 cP @Temperature 75.0 °F |
#3 spindle @ 20 rpm; ASTM D2393 |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |