Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2900 - 3700 cP | 2900 - 3700 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/33 Linear Thermoplastic Polyurethane Pearlstick D40-70/33 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. S.. |