Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2360 cP @Temperature 23.9 °C |
2360 cP @Temperature 75.0 °F |
1 minute |
BCC Products Kwik Kast BC 8650 Urethane Casting BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl.. |