Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 15000 - 23000 cP @Temperature 25.0 °C |
15000 - 23000 cP @Temperature 77.0 °F |
Spindle CP52 @ 10rpm |
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle.. |