Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 22.76 cP | 22.76 cP | 25% by weight in toluene; ASTM D445 |
KKPC KOSYN KTR 401 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |