Polymer Property : Brookfield Viscosity = 17590 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 17590 cP

@Temperature -40.0 °C
17590 cP

@Temperature -40.0 °F
ASTM D2983
ExxonMobil SpectraSyn™ 8 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) ..