Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1650 cP @Temperature 160 °C |
1650 cP @Temperature 320 °F |
ETM E-31 |
ExxonMobil ESCOREZ™ 1102RM (Europe) Petroleum Hydrocarbon Resin Aliphatic hydrocarbon resin specifically designed as a binder for thermoplastic road marking formulations. Availability: Africa & Middle East and EuropeInformation provided by ExxonMobil Chemical |