Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 160000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #10 sp @ 2 rpm
3M AC-236 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #10 sp @ 2 rpm
3M AC-236 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #7 sp @ 2 rpm
3M AC-236 Class C-20 Aerospace Sealant
3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance ..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #7 sp @ 2 rpm
3M AC-236 Class C-80 Aerospace Sealant
3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance ..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #10 sp @ 2 rpm
3M AC-275 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #10 sp @ 2 rpm
3M AC-275 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #10 sp @ 2 rpm
3M AC-275 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #7 sp @ 10 rpm
3M AC-645 B-2 Aerospace Sealant
3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli..
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #10 sp @ 2 rpm
3M AC-236 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Copyright © lookpolymers.com All Rights Reserved