Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | <= 15 cP | <= 15 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 156 Nonionic carnauba wax emulsion Description: Nonionic carnauba wax emulsionUsage: Michem® Lube 156 can be used as an additive in polishes (specifically car polish), cosmetics, paints, coatings and graphic arts to increase scrat.. |
|||
Brookfield Viscosity | <= 15 cP | <= 15 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 160F Anionic carnauba wax emulsion Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160F provides superior slip and mar resistance on a variety of substrates such as metal, wood, film and paper. Anti-block properties .. |
|||
Brookfield Viscosity | <= 15 cP | <= 15 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 160PF Anionic carnauba wax emulsion Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160PF is an APEO-free additive which imparts slip, abrasion resistance and anti-block properties, in a variety of coatings and varnis.. |
|||
Brookfield Viscosity | <= 15 cP | <= 15 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 160PFP Anionic carnauba wax emulsion Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160PF is an APEO-free additive which imparts slip, abrasion resistance and anti-block properties, in a variety of coatings and varnis.. |
|||
Brookfield Viscosity | <= 15 cP | <= 15 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 182 Anionic carnauba/paraffin wax emulsion Description: Anionic carnauba/paraffin wax emulsionUsage: Michem® Lube 182 can provide slip, release and anti-block properties in a number of applications ranging from wood coatings to being blen.. |
|||
Brookfield Viscosity | <= 15 cP | <= 15 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 160 Anionic carnauba wax emulsion Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160 provides superior slip and mar resistance on a variety of substrates such as metal, wood, film and paper. Anti-block properties a.. |
|||
Brookfield Viscosity | 15 cP | 15 cP | #1 spindle; 6 rpm. |
DuPont Performance Polymers Neoprene 571 Polychloroprene
(discontinued **) Main feature: High tensile strength. Principal uses include: Dipped goods, Elasticized concrete, Adhesives (Cord) Coatings.Solids content: 50%. Initial pH: 12. Surface tension: 40 dyne/cm. Polym.. |
|||
Brookfield Viscosity | 15 cP | 15 cP | #1 spindle; 30 rpm. |
DuPont Performance Polymers Neoprene 571 Polychloroprene
(discontinued **) Main feature: High tensile strength. Principal uses include: Dipped goods, Elasticized concrete, Adhesives (Cord) Coatings.Solids content: 50%. Initial pH: 12. Surface tension: 40 dyne/cm. Polym.. |
|||
Brookfield Viscosity | 15 cP | 15 cP | #1 spindle; 30 rpm. |
DuPont Performance Polymers Neoprene 842A Polychloroprene
(discontinued **) Fast curing. Principal uses include: Treated paper, Bonded fibers, Dipped goods, Coatings, Elasticized concrete, Carpet backing, Adhesives (Lamination).Solids content: 50%. Initial pH: 12. Surfac.. |
|||
Brookfield Viscosity | 15 cP | 15 cP | #1 spindle; 6 rpm. |
DuPont Performance Polymers Neoprene 842A Polychloroprene
(discontinued **) Fast curing. Principal uses include: Treated paper, Bonded fibers, Dipped goods, Coatings, Elasticized concrete, Carpet backing, Adhesives (Lamination).Solids content: 50%. Initial pH: 12. Surfac.. |