Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 14500 cP @Temperature 25.0 °C |
14500 cP @Temperature 77.0 °F |
|
Loctite® 3336 Epoxy Light Cure Adhesive Epoxy Light Cure AdhesivesLoctite® 3336 Epoxy Light Cure AdhesiveA UV cure, medium viscosity two-part epoxy. UV cure effects fast gellation. Complete cure at room temperature or heat cure. Tough an.. |