Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 145 cP @Temperature 25.0 °C |
145 cP @Temperature 77.0 °F |
Extrusion rate, grams/minute, 1/8" orifice at 90 psi |
Loctite® 5083 Silicone Light Cure Adhesive Silicon Light Cure AdhesivesLoctite® 5083 Silicone Light Cure Adhesive Key Substrates: Glass, Metal, Ceramic Cure Type: Ultraviolet, Moisture, Methoxy Bonding Type: Silicon |