Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 12500 cP | 12500 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 24A PVC PVC Homopolymer Dispersion Resin F-24A is a low molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compounds as well as other applica.. |