Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 118000 cP @Temperature -26.0 °C |
118000 cP @Temperature -14.8 °F |
|
ChevronTexaco Havoline® SAE 80W-90 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Brookfield Viscosity | 118000 cP @Temperature -26.0 °C |
118000 cP @Temperature -14.8 °F |
|
ChevronTexaco Multigear® EP SAE 80W-90 Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties.. |
|||
Brookfield Viscosity | 118000 cP @Temperature -26.0 °C |
118000 cP @Temperature -14.8 °F |
|
ChevronTexaco RPM® SAE 80W-90 Universal Gear Lubricant FeaturesChevron RPM Universal Gear Lubricants are multipurpose lubricants.They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protecti.. |