Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1.10e+7 - 1.80e+7 cP @Temperature 25.0 °C |
1.10e+7 - 1.80e+7 cP @Temperature 77.0 °F |
6 rpm or 3 rpm depending on viscosity |
DuPont Performance Polymers Neoprene AD-5 Polychloroprene Rubber
(discontinued **) Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development. More color-stable than neoprene AC during storage.Processing and .. |