Brookfield Viscosity 1.25e+8 - 1.75e+8 cP

@Temperature 25.0 °C
1.25e+8 - 1.75e+8 cP

@Temperature 77.0 °F
6 rpm or 3 rpm depending on viscosity
DuPont Performance Polymers Neoprene ADQ 55 Polychloroprene Rubber  (discontinued **)
Description: Fast dissolving, good rheology chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development. More color-stable than Neoprene AC..