Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 950000 - 1.30e+6 cP | 950000 - 1.30e+6 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-770 Class B-1 Aerospace Sealant 3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio.. |
|||
Brookfield Viscosity | 950000 - 1.30e+6 cP | 950000 - 1.30e+6 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-770 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio.. |
|||
Brookfield Viscosity | 900000 - 1.30e+6 cP | 900000 - 1.30e+6 cP | Base, RVF #6 sp @ 2 rpm |
3M AC-250 B-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read.. |