Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 0.60 cP | 0.60 cP | 25% in toluene; ASTM D2994 |
Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS) Solprene 9618 is a 69/31 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It is stabilized with non-staining antioxidant system. This product is presented as a free flowing po.. |