Physical Properties | Metric | English | Comments |
---|---|---|---|
Soluble Sulfates | 250 ppm | 250 ppm | |
Old Hickory S-4 Tennessee Ball Clay The S-4 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous compositions. It has excellent response to deflocculation and very good casting rate while ma.. |