Physical Properties | Metric | English | Comments |
---|---|---|---|
Soluble Sulfates | 192 ppm | 192 ppm | |
Old Hickory Dunn Tennessee Ball Clay Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an.. |