Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 96 hour | >= 96 hour | Condition B, F20, 100% Igepal; ASTM D1693 |
Ineos TC46-25 HDPE TC46-25 is a natural high density polyethylene copolymer designed specifically for telecommunications ducting to meet or exceed the material requirements in ASTM F2160, UL 651B and MEMA TC-7. TC46-.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Visico™ LE4421/LE4438 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ LE4421 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Visico™ LE4421M/LE4431M Polyethylene Visico™ LE4421M / Visico™ LE4431M is a two-part silane crosslinkable insulation system, specially designed for insulation applications. Applications: Visico™ LE4421M / Visico™ LE4431M is intend.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Visico™ LE4423/LE4438 Polyethylene Compound, Crosslinkable Visico™ LE4423 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ LE4423 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Visico™ ME4425/LE4438 Polyethylene Visico™ ME4425 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ ME4425 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE442.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 100%; F20; IEC 60811-4-1/B |
Borealis LE6006 Polyethylene It is a low loss LDPE compound for coaxial cables. LE6006 contains a special type of antioxidant, which does not adversely affect the electrical properties. Applications: bamboo constructed cables,.. |
|||
Environmental Stress Crack Resistance | >= 96 hour @Temperature 50.0 °C |
>= 96 hour @Temperature 122 °F |
Igepal 10%, F20; IEC 60811-4-1/B |
Borealis Visico™/Ambicat™ LE4421/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4476 is a silane crosslinkable natural compound designed for low voltage power cables up to 6kV. The base material Visico™ LE4421 in combination with the catalyst mas.. |