Polymer Property : Environmental Stress Crack Resistance = 8.00 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance 8.00 - 1000 hour
8.00 - 1000 hour
Average value: 373 hour Grade Count:19
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m..