Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 75 hour | 75 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 59E HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 75 hour | 75 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 59F HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 75 hour | 75 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |