Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 60 hour | >= 60 hour | ISO 22088 |
Polimeri Europa Eraclene® BC 82 High Density Polyethylene - Blow Molding Eraclene BC 82 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Environmental Stress Crack Resistance | 60 hour | 60 hour | Condition B, F50; ASTM D1693 |
IRPC Polimaxx Polene G2855 High Density Polyethylene CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI.. |
|||
Environmental Stress Crack Resistance | 60 hour @Temperature 50.0 °C |
60 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1693 |
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App.. |
|||
Environmental Stress Crack Resistance | 60 hour | 60 hour | F50, Anatarox 100%; ASTM D 1693B |
Total HDPE 5502 R3 High Density Polyethylene - Blow Molding HDPE 5502 R3 is a high density polyethylene with good compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of blow molded pa.. |
|||
Environmental Stress Crack Resistance | 60 hour | 60 hour | FNCT; ISO 16770 |
Total XSene® 55060 High Density Polyethylene - Blow Molding HDPE 55060 is a semi high molecular weight (SHMW) high density polyethylene with outstanding Environmental Stress Crack Resistance and rigidity. It has been specifically designed for the manufactur.. |