Polymer Property : Environmental Stress Crack Resistance = 550 hour
Polymer Property :
Environmental Stress Crack Resistance =
550 hour
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Environmental Stress Crack Resistance
550
hour
550
hour
JPJ Technologies 8300B HDPE Blow Molding
Information provided by JPJ Technologies