Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 48 hour | 48 hour | F<sub>50</sub>; Condition B, 100% Igepal; ASTM D1693 |
NOVA Chemicals Novapol® HB-L354-A HDPE Blow Molding Resin Good balance of physical and molding properties-high toughness, Excellent processability on high-speed, multiple-head blow molding lines, UL-94HB listedApplications: Household chemical bottles, Indu.. |
|||
Environmental Stress Crack Resistance | >= 48 hour @Temperature 50.0 °C |
>= 48 hour @Temperature 122 °F |
Igepal 10%; F20; IEC 60811-4-1/B |
Borealis HE3366 High Density Polyethylene HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer sk.. |
|||
Environmental Stress Crack Resistance | 48 hour | 48 hour | F<sub>o</sub>; Compression molded parts prepared according to ASTM D 1928, condition B.; ASTM D1693 |
Dow DGDA-2475 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the.. |